Characteristic Assessment of Stabilized Polyacrylonitrile Nanowebs for the Production of Activated Carbon Nano-Sorbents

S. Rafiei B. Noroozi Sh. Arbab A.K. Haghi

Citation:  S. Rafiei, B. Noroozi, Sh. Arbab, A.K. Haghi. Characteristic Assessment of Stabilized Polyacrylonitrile Nanowebs for the Production of Activated Carbon Nano-Sorbents[J]. Chinese Journal of Polymer Science, 2014, 32(4): 449-457. doi: 10.1007/s10118-014-1410-4 shu

Characteristic Assessment of Stabilized Polyacrylonitrile Nanowebs for the Production of Activated Carbon Nano-Sorbents

    通讯作者: B. Noroozi,
摘要: Polyacrylonitrile (PAN) nanofibers with average diameter of 300 nm were produced by electro-spinning. The nanofibers were stabilized at different temperatures in the range of 180-270 ℃ in several duration times and heating rates. Fourier transforms infrared (FTIR) spectroscopy, differential scanning calorimetry (DSC) and X-ray diffraction (XRD) analyzing techniques were employed to measure the extent of stabilization reaction. By all procedures, the ranges of temperature and duration time recommended were about 250-270 ℃ and 1-2 h, respectively. Increasing the activation temperature from 800 ℃ to 1200 ℃ caused porosity and pore volume development up to 60% and 0.532 cm3/g, respectively. Pore width of all samples was calculated to be about 0.7 nm confirming micro-pore structure of the produced PAN based activated carbon nanofibers. Comparing dye adsorption for different adsorbents including chitin and granular activated carbon (GAC) showed the highest efficiency for the produced activated carbon nanofibers (ACNFs).

English


    1. [1]

      Lee,S.,Koeran J.Chemi.Eng,2010,27.10[2]Mostafavia, S., Mehrnia, M. and Rashidi, A., Desalination, 2009, 238:88[3]Lozano-Castello, D., Cazorla-Amoros, D[J].and Linares-Solano, A., Energy Fuel.2002, 16:1321-[4]Poole.[J].C. and Owens, F., Introduction to Nanotechnology, John Wiley Sons, Inc, Hoboken, New Jersey.2003,:-[5]Thavasi, V., Singh, G[J].and Ramakrishna, S., Energy Environ. Sci.2008, 1:205-[6]Wang.[J].Z. L., Nanomaterials for Nanoscience and Nanotechnology, Wiley-VCH Verlag GmbH, Weinheim.2000,:-[7]Kim, C., Ngoc, B., Yun, W., Lee, J. and Yang, K., Carbon, 2008, 42:34[8]Oh, G., Ju, Y[J]., Jung, H. and Lee, W., J. Anal. Appl. Pyrol.2008, 81:211-[9]Khanna, V., Bakshi, B. R. and James Lee, L., J. Ind. Ecol., 2008, 12:394[10]Kim, D., Park, S., Kim, B., Chin, B., Jo, S. and Kim, D., Macromol. Res., 2005, 13:521[11]Ali, A., and El-Hamid, M[J]., Compos. A. Appl. Sci.2006, 37:1681-[12]Lai, C., Zhong, G., Yue, Z., Chen, G., Zhang, L., Vakili, A., Wang, Y., Zhu, L., Liu, J. and Fong, H., Polymer, 2011, 52:519[13]Yusof, N. and Ismail, A., J. Anal. Appl. Pyrolysis., 2011, 93:1[14]Mukesh, K. J., and Balasubramanian, M[J]., J. Mater. Sci.1987, 22:301-[15]Gu, S., Ren, J[J].and Vancso, G., Euro. Polym. J.2005, 41:2559-[16]Blackman, J., Patrick, J., Arenillas, A., Shi, W. and Snape, C., Carbon, 2006, 44:44[17]Su, Y., Ko, T[J].and Lin, J., J. Appl. Polym. Sci.2008, 108:3610-[18]Bhardwaj, N. and Kundu, S[J].C., Biotechnol. Adv.2010, 28:325-[19]Fazlitdinova, A., Tyumentsev, Podkopayev, V. S. and Shveikin, G., J. Mater. Sci., 2010, 45:3998[20]Nataraj, S., Yang, K[J].and Aminabhavi, T., Prog. Polym. Sci.2012, 37:487-[21]Reneker, D. and Chun, I[J]., Nanotechnol.1996, 7:216-[22]Arshad, S., Naraghi, M. and Chasiotis, I., Carbon, 2011, 49:1710[23]Panapoy, M., Dankeaw, A. and Ksapabutr, B., Thammasat Int. J. Sci. Tech., 2008, 13:11[24]Wu, M., Wang, Q[J]., Li, K., Wu, Y. and Liu, H., Polym. Degrad. Stabil.2012, 97:1511-[25]Wu, G. P., Lu, C. X., Ling, L. C. and Lu, Y.G., Polym. Bull., 2009, 62:667[26]Belyaev, S. S., Arkhangelsky, I. V. and Makarenko, I. V., Thermochim. Acta, 2010, 507:9[27]Esrafilzadeh, D., Morshed, M[J].and Tavanai, H., Synthetic Met.2009, 159:267-[28]Hearle.[J].J. W. S., High Performance Fibers, Woodhead Publishing Ltd, North and South America.2001,:-[29]Heikkil, P. and Harlin, A[J]., Express Polym. Lett.2009, 3:437-[30]Ziabari, M., Mottaghitalab, V[J].and Haghi, A. K., Korean J. Chemi. Eng.2010, 27:340-[31]Wangxi, Z., Jie, L[J].and Gang, W., Carbon.2003, 41:2805-[32]Shimada, I. and Takahagi, T[J]., J. Polym. Sci. A. Polym. Chem.1986, 24:1989-[33]Ouyang, Q., Cheng, L[J]., Wang, H. and Li, K., Polym. Degrad. Stabil.2008, 93:1415-[34]Kaburagi, M., Bin, Y., Zhu, D., Xu, C. and Matsuo, M., Carbon, 2003, 41:915[35]Yu, M., Wang, C., Bai, Y., Wang, Y., Wang, Q. and Liu, H. Polym. Bull., 2006, 57:525[36]Yu, M., Bai,Y., Wang, C., Xu, Y. and Guo, P., Mater. Lett., 2007, 61:2292

  • 加载中
计量
  • PDF下载量:  0
  • 文章访问数:  2066
  • HTML全文浏览量:  225
文章相关
  • 发布日期:  2014-04-05
  • 收稿日期:  2013-07-04
  • 修回日期:  2013-09-02
通讯作者: 陈斌, bchen63@163.com
  • 1. 

    沈阳化工大学材料科学与工程学院 沈阳 110142

  1. 本站搜索
  2. 百度学术搜索
  3. 万方数据库搜索
  4. CNKI搜索

/

返回文章